Simulation of Flotation Plants

For a greenfield plant design, the flotation models are typically based on kinetic laboratory tests carried out both for the rougher and cleaner stag It is also common to carry out closed loop locked cycle laboratory tests and pilot...

Froth Flotation Process

Flotation behaviour of arsenic and non-arsenic copper minerals at finer sizes was investigated by grinding and flotation tests conducted in the on-site laboratory at Rosebery on samples taken from the copper rougher concentrate...

Copper Flotation

2017/03/19· Although a clean rougher tailing can often be achieved at 65-mesh the copper mineral is not liberated sufficiently to make a high grade copper concentrate, thus some form of regrinding is necessary on the rougher flotation copper...

Recovery of pyrite from copper tailings by flotation

The rougher flotation tests were performed in a Denver D-12 flotation machine with a 25 L cell In each rougher flotation test, 2260 L of fresh tailing pulp with 374 ± 13% solid by weight, 47 ± 03% pyrite grade, and pH 96 ± 04...